ASTM A202锅炉容器板化学成分:
ASTM A202 |
化学元素含量(上限 %) |
|||||
C | Si | Mn | P | S | Cr | |
A级 | 0.17 | 0.54-0.96 | 0.97-1.52 | 0.035 | 0.035 | 0.31–0.64 |
B级 | 0.25 | 0.54-0.96 | 0.97-1.52 | 0.035 | 0.035 | 0.31–0.64 |
ASTM A202锅炉容器板力学性能:
ASTM A202 | A级 | B级 |
抗拉强度, kis [MPa] | 75-95 [515-655] | 85-110 [585-760] |
屈服度, kis [MPa] | 45 [310] | 47 [325] |
伸长率,标距8 in. [200 mm], % | ≧16 | ≧15 |
伸长率,标距2 in. [50 mm], % | ≧19 | ≧18 |
ASTM A202锅炉容器板广泛应用于石油、天然气工程项目中,用于制造压力容器、锅炉、储罐和换热器等设备。